Отпуск в масле углеродистой стали SAE1070-1090
UNS: G10600-10900 DIN: 1.1231-1.1248 GB: 65Mn、70Mn Modulus of elasticity: 206843 Recommended maximum operating temperature: 121 °C Main element chemical composition (wt%):C0.65 – 0.98%, Mn 0.30 –
Углеродистая сталь SAE1060-1080 (холодная вытяжка или холодная прокатка)
UNS: G10600-10900 DIN: 1.1231-1.1248 GB: C58D-C88D Modulus of elasticity: 206843 Recommended maximum operating temperature: 121 °C Main element chemical composition (wt%):C 0.55 – 0.88, Mn 0.40-0.90%
Монель К-500
UNS: N05500 DIN: 2.4375 GB: 68Ni28Cu28Al Modulus of elasticity: 179140 Recommended maximum operating temperature: 287 °C Main element chemical composition (wt%):Ni 63.0 min%, Cu 27.0 -33.0%,
Монель K-400
UNS: N04400 DIN: 2.436 GB: 68Ni28Cu28Fe Elastic modulus: 179140 Recommended maximum operating temperature: 232°C Main element chemical composition (wt%) : Ni 63.0min %, Cu 28.0-34.0% Description
Хастеллой C-276
UNS: N10276 DIN: 2.4819 GB: NS3304 Elastic modulus: 211523 Recommended maximum operating temperature: 371°C Major element chemical composition (wt %) : 51.0 63.5% Ni, Cr 14.5
Инконель 718
UNS: N07718 DIN: 2.4668 GB: GH4169 Модуль упругости: 204085 Рекомендуемая максимальная рабочая температура: 704°C Химический состав основных элементов (wt%) : Ni 50.0-55.0%, Cr 17.0-21.0%, Fe11.0-24.0% Описание
Инконель Х-750
UNS: N07750 DIN: 2.4669 GB: GH4145 Модуль упругости: 213737 Рекомендуемая максимальная рабочая температура: 371(538)°C Химический состав основных элементов (wt%) : Ni70.0min %, Cr 14.0-17.0%, Fe 5.0-9.0%
Экзотические сплавы A-286
UNS: S66286 DIN: 1.498 GB: GH2132 Модуль упругости: 213737 Рекомендуемая максимальная рабочая температура: 538°C Химический состав основных элементов (мас.%) : NI 24-27%, 13.5 16.0% Cr,